Teeb meem Carbonate Buildup
Cyanide tooj liab plating da dej sau cov ntsev carbonate dhau sijhawm. Sodium carbonate thiab potassium carbonate daim ntawv los ntawm kev nqus ntawm atmospheric carbon dioxide los ntawm cov alkaline da dej (pH 12-13). Cov tshuaj tiv thaiv yog: 2NaOH + CO₂ → Na₂CO₃ + H₂O. Cov carbonate concentration nce maj mam los ntawm kev ua haujlwm da dej.
Qhov teeb meem nrawm nrawm ntawm lub tshuab cua sov. Cov cua sov ua kom sov, nrog rau phab ntsa kub ntawm 80-100 degree, tsim cov cheeb tsam hauv cheeb tsam uas cov carbonate solubility ntau dhau. Carbonate precipitates raws li ib qho nyuaj, crystalline nplai ntawm lub raj nto. Cov nplai insulates cov hlab, txo cov cua sov hloov mus, thiab nws thiaj li yuav tsum tau siv tshuab lossis tshuaj descaling. Cov txheej txheem descaling- feem ntau yog siv hydrochloric acid-tsim cov khoom pov tseg thiab siv sijhawm ntau lawm.
Lub tshuab hluav taws xob PTFE ua haujlwm ntawm phab ntsa qis (55-70 degree), qhov twg cov carbonate solubility siab dua. Cov nag lossis daus ntawm lub raj saum npoo yog txo qis. Cov carbonate tseem yaj hauv cov da dej ntau, qhov uas nws tuaj yeem tswj tau los ntawm cov txheej txheem khov-tawm los yog nag lossis daus, tsis yog tsim rau ntawm lub tshuab cua sov.
Qhov kub thiab txias -Dependent Solubility Mechanism
Sodium carbonate solubility hauv dej yog qhov kub thiab txias -nyob ntawm. Ntawm 30℃(ib txwm da dej kub rau cyanide tooj liab), solubility yog kwv yees li 50 g / 100 mL. Ntawm 80℃(hlau rhaub phab ntsa kub), cov solubility poob rau kwv yees li 45 g / 100 mL. Ntawm 95℃(titanium rhaub phab ntsa kub), nws poob ntxiv mus rau kwv yees li 42 g / 100 mL.
Lub da dej ntawm 30℃tej zaum yuav qis dua cov carbonate saturation txwv. Cov txheej txheej nyias nyias ntawm lub tshuab cua sov, rhuab mus rau 80-95 degree, tshaj qhov kev txwv hauv zos saturation. Carbonate precipitates ncaj qha mus rau lub raj nto. Cov nag lossis daus tsis tu ncua ntev li ntev tau ntev npaum li lub da dej muaj cov carbonate yaj thiab lub tshuab cua sov tswj qhov siab ntawm phab ntsa.
PTFE qhov kub ntawm phab ntsa qis (55-70 degree) ua kom cov ciam teb nyob ze rau qhov kub da dej. Lub solubility ntawm 60℃yog kwv yees li 47 g / 100 mL-ze rau cov nqi ntau thiab tsis tshua muaj siab tshaj saturation. Lub zog tsav los nag yog txo los ntawm 50-70%.
| Carbonate Parameter | Stainless hlau rhaub | Titanium rhaub | PTFE Thaum tshav kub kub Exchanger |
|---|---|---|---|
| Phab ntsa kub ntawm 3 barg chav (degree) | 80-95 | 85-100 | 55-70 |
| Na₂CO₃ solubility ntawm phab ntsa kub (g / 100mL) | 44-45 | 42-44 | 47-48 |
| kwv tij nag xob nag cua tsav zog | 1.0 (lub hauv paus) | 1.1-1.3 | 0.3-0.5 |
| Carbonate scale tsim tus nqi | Siab | Siab | Tsawg |
| Descaling zaus | 6-12 lub lis piam | 4-10 lub lis piam | 12-24 lub hlis |
PTFE Surface Synergy
PTFE lub zog nto qis (18-20 mN / m) muab kev tiv thaiv theem nrab tiv thaiv carbonate scaling. Txawm tias thaum nag lossis daus tshwm sim, cov crystals adhere tsis muaj zog rau hydrophobic PTFE nto. Cov crystals yog dislodged los ntawm ib txwm da dej ncig los yog agitation. Lawv tsis tsim nyob rau hauv ib qho nyuaj, mechanically interlocked nplai txheej uas ua rau ntawm cov hlau nplaum.
Kev sib xyaw ua ke ntawm cov nag lossis daus tsav tsheb (los ntawm qhov kub ntawm phab ntsa) thiab txo qhov adhesion (los ntawm lub zog qis) ua rau PTFE tiv taus carbonate scaling hauv cyanide tooj liab kev pab cuam. Lub sijhawm descaling ncua ntawm lub lis piam mus rau lub hlis lossis xyoo.
Bath Chemistry Management Benefit
Cov pa roj carbon monoxide nyob rau hauv lub da dej yog tswj los ntawm lub caij ntuj sov khov - tawm - txias ib feem ntawm lub da dej kom crystallize carbonate, uas yog lim tawm - los yog los ntawm cov tshuaj los nag nrog calcium hydroxide. Cov txheej txheem no tau ua nyob rau hauv ntau lub da dej thiab tsis cuam tshuam los ntawm kev xaiv cov khoom siv hluav taws xob.
Qhov zoo ntawm PTFE yog cov carbonate tseem nyob hauv cov da dej ntau, qhov uas nws tuaj yeem tswj tau los ntawm cov txheej txheem no, tsis yog tso rau ntawm lub tshuab cua sov qhov chaw uas nws ua rau kub hloov pauv thiab yuav tsum tau sib cais, nruj dua descaling. Kev saib xyuas da dej ua kom pom tau ntau dua thiab tsis tshua muaj.
Cov ntsiab lus
Cyanide tooj liab da dej tsim cov carbonate sludge rau ntawm cov khoom siv hluav taws xob hlau vim qhov txo cov carbonate solubility ntawm phab ntsa kub (80-100 degree). PTFE kub exchangers, nrog rau lawv sab phab ntsa kub (55-70 degree), txo cov nag los nag los ntawm 50-70%. Lub zog qis PTFE nto ntxiv inhibits crystal adhesion. Carbonate tseem nyob hauv cov da dej ntau, qhov uas nws tau tswj hwm los ntawm cov txheej txheem niaj hnub, tsis yog tsim cov nplai insulating ntawm lub rhaub.
Kev txhawb nqa engineering rau PTFE heat exchanger specification nyob rau hauv cyanide thiab alkaline plating da dej yog muaj nyob rau ntawm xa mus rau da dej chemistry, kev khiav hauj lwm kub, tam sim no descaling zaus, thiab carbonate cov txheej txheem.