Lub pas dej ntawm cov txheej txheem dej nyob rau hauv lub tshav kub exchanger los yog ib tug spike nyob rau hauv conductivity nyob rau hauv dej txias qhia lub raj xau. Kev kaw tag nrho cov kab yuav raug nqi ntau txhiab ib feeb. Ob peb qhov chaw nres tsheb xwm txheej ceev tuaj yeem cais cov xau thiab ua kom cov nroj tsuag khiav mus txog rau lub sijhawm kho qhov rai tom ntej. Rau PTFE plhaub-thiab- tube exchangers, aThaum muaj xwm ceev kho tubesheet xau PTFE exchangertxheej txheem feem ntau suav nrog kev txheeb xyuas lub raj xau thiab ntsaws ob qhov kawg, lossis -tej zaum tsis tshua muaj nyob ntawm cov ntawv sib koom ua ke - siv lub clamp sab nraud ib ntus. Cov kev ntsuas no tsis yog cov kev daws teeb meem mus tas li, tab sis lawv tuaj yeem tiv thaiv qhov kev puas tsuaj loj los ntawm kev yuam kom muaj kev puas tsuaj tam sim ntawd.
Paub txog Tubesheet lossis Tube Leak hauv PTFE Exchanger
PTFE cov khoom siv hluav taws xob sib txawv yog cov corrosion heev-resistant, tab sis cov neeg kho tshuab puas tsuaj-xws li kev co, raj-rau- baffle hnav, los yog kev teeb tsa tsis raug- tuaj yeem ua rau cov pa xau ntawm lub raj xaim sib koom lossis lub pinhole hauv ib lub raj. Cov cim qhia txog kev xau muaj xws li:
Pom dej ntws tawmlos ntawm lub plhaub -sab ntws, qhov cua, lossis flange pob qij txha
Unexplained poob ntawm cov txheej txheem kualos yog txias nruab nrab
Conductivity lossis pH hloovnyob rau hauv dej txias (lub plhaub sab) thaum txheej txheem dej yog aqueous
Siab lwjnyob rau hauv ob lub raj sab los yog plhaub sab thaum lub sij hawm niaj hnub kuaj
Leaks tuaj yeem tshwm sim hauv ob qhov chaw:
Tube-rau-tubesheet sib koom- qhov twg PTFE raj yog nthuav los yog welded rau hauv PTFE los yog hlau tubesheet
Tube phab ntsa nws tus kheej- ib tug pinhole los yog tawg nyob rau hauv lub PTFE raj lub cev
Cov lus teb thaum muaj xwm txheej kub ntxhov txawv me ntsis nyob ntawm qhov chaw xau, tab sis lub raj ntsaws yog qhov kev txhim kho tseem ceeb rau ob qho xwm txheej, yog tias qhov xau yog nyob rau sab raj.
Kauj Ruam 1: Txheeb xyuas lub raj xa dej yam tsis muaj kev cuam tshuam tag nrho
Ua ntej txhua qhov ntsaws lossis clamping tuaj yeem ua tau, lub raj xa dej yuav tsum raug txheeb xyuas. Kev kaw tag nrho cov khoom sib pauv feem ntau yog yuav tsum tau nkag mus rau hauv cov tubesheets, tab sis lub hom phiaj yog kom txo lub sijhawm poob qis dua - tsis txhob zam kev kaw tag nrho. Thaum lub exchanger raug cais tawm ntawm cov txheej txheem thiab ntws, cov hauv qab no yog siv:
Kev ntsuam xyuas hydrostatic.Lub plhaub sab yog ntim nrog dej lossis lwm cov kua dej sib xyaw ua ke, thiab lub raj sab yog pressurized nrog cua lossis nitrogen. Cov tshuaj xab npum yog siv rau txhua lub raj kawg ntawm lub tubesheet. Npuas ntawm ib lub raj tshwj xeeb qhia txog qhov xau. Tsis tas li ntawd, lub plhaub sab yog pressurized, thiab lub raj xaus yog pom rau kev tshem tawm dej.
Tracer gas method.Lub helium leak detector los yog halogen tracer gas yog nkag mus rau ib sab, thiab ib tug sniffer sojntsuam yog siv ntawm txhua lub raj kawg. Qhov no sai dua rau cov pob khoom loj.
Visual tshuaj ntsuam nrog borescope.Yog tias qhov xau loj txaus, lub borescope tso rau hauv lub raj tuaj yeem pom cov kab nrib pleb lossis qhov hauv PTFE phab ntsa.
Thaum lub raj xa dej raug txheeb xyuas, nws qhov chaw nyob (kab, kab, thiab txoj hauj lwm hauv lub nras) raug kaw. Lub hom phiaj yog kom nres qhov xau yam tsis muaj kev hloov tam sim ntawm tag nrho cov raj ntim.
Kauj Ruam 2: Tube Plug - Tus Txheej Txheem Kho Thaum Muaj Xwm Ceev
Tube ntsaws yog cov txheej txheem xwm txheej ceev tshaj plaws thiab txhim khu kev qha rau lub raj xau hauv lub plhaub PTFE-thiab- tube exchanger. Lub raj xau yog kaw tas li ntawm ob qho kawg, tiv thaiv kev ntws los ntawm lub raj ntawd. Cov txheej txheem cov kua dej txuas ntxiv ntws mus los ntawm cov hlab ntsha uas muaj kev noj qab haus huv, thiab lub plhaub - sab cua txias lossis cua sov nruab nrab tsis muaj kev cuam tshuam tshwj tsis yog rau qhov me me ntawm qhov chaw hloov hluav taws xob.
Yuav tsum tau cov cuab yeej thiab cov khoom siv
Cov khoom siv ntsaws yuav tsum tau khaws cia rau ntawm -qhov chaw rau PTFE exchangers tseem ceeb. Cov khoom siv muaj:
Tapered PTFE los yog PFA plugs- qhov loj me tshwj xeeb rau qhov nominal puab txoj kab uas hla (ID) ntawm PTFE hlab. Feem ntau muaj rau tube IDs ntawm 6 mm txog 25 mm.
Ib tug mos- ntsej muag mallet( tooj dag, nylon, lossis roj hmab) rau tapping ntsaws rau hauv qhov chaw.
Tube- kawg deburring cuab tamtshem tawm tej burrs los yog irregularities.
Sealant (yeem)- PTFE muab tshuaj txhuam los yog fluoropolymer - tau tshaj xov sealant rau kev ruaj ntseg ntxiv.
Plug txheej txheem
Ntxuav lub raj kawg.Tube ID ntawm ob lub ntsej muag tubesheet yuav tsum tsis muaj khib nyiab, deposits, los yog corrosion. Siv ib lub txhuam txhuam los yog ib tug mos reamer, saib xyuas kom tsis txhob khawb PTFE nto.
Ntxig lub tapered plugmus rau hauv lub raj kawg nrog lub taub me me nkag mus ua ntej. Lub ntsaws yuav tsum me ntsis loj dua piv rau lub raj ID.
Coj mus rhaub maj mam nrog lub malletkom txog thaum lub ntsaws ruaj ruaj. Lub ntsaws yuav tsum protrude me ntsis los ntawm lub ntsej muag tubesheet tab sis tsis ntev mus tob rau hauv lub raj. Kev sib txhuam haum yog tsim los ntawm elastic deformation ntawm PTFE.
Rov ua dua rau ntawm qhov opposite tubesheet.Ob qhov kawg ntawm tib lub raj yuav tsum tau ntsaws kom tsis txhob muaj kev hla dhau.
Tom qab ntsaws, qhov ntsuas cua qis - tuaj yeem ua rau ntawm lub plhaub sab kom paub meej tias qhov xau tau nres. Yog hais tias lub plug yog xoob, ib tug me ntsis loj plug los yog ib tug thib ob plug tsav nyob rau hauv qab thawj yuav siv tau.
Kev txiav txim siab tseem ceeb rau kev ntsaws
PTFE dej txias.PTFE paub tias nkag los yog txias - ntws raws li kev ntxhov siab compressive. Nyob rau tib lub sijhawm, lub ntsaws ntsaws ruaj ruaj tuaj yeem so me ntsis. Vim li no, qee phau ntawv qhia txog kev saib xyuas pom zoo kom rov-tapping lub ntsaws tom qab 24 teev ua haujlwm.
Txo tshav kub hloov chaw.Txhua lub raj ntsaws tshem tawm lub raj ntawd qhov kev pab cuam rau tag nrho cov cua sov hloov mus. Ob peb lub raj txuas (feem ntau txog li 5-10% ntawm cov pob khoom) muaj qhov cuam tshuam tsis zoo rau kev ua haujlwm, yog tias lub exchanger tsis tau khiav ntawm nws lub peev xwm siab tshaj plaws. Txawm li cas los xij, yog tias muaj ntau lub raj txuas, cov nqi tsim khoom yuav tsum raug txo kom tswj qhov hluav taws xob kub.
Flow Distribution cuam tshuam.Plug ib lub raj hloov pauv qhov sib npaug ntawm hydraulic hla lub raj, tab sis nrog ob peb lub ntsaws, qhov cuam tshuam ntawm kev faib tawm yog tsawg heev. Randomly faib plugs yog zoo dua li clustering plugs nyob rau hauv ib cheeb tsam.
Kauj Ruam 3: Lwm Txoj Kev Kho Ib Nrab - Sab Nraud Split Clamp rau Tubesheet Joint Leaks
Yog tias cov pa xau tuaj ntawm lub raj - mus rau - tubesheet sib koom ua ke (tsis yog lub raj phab ntsa), thiab yog tias lub raj xaim siv tau, ib qho tshwj xeeb tsimcais-clamptuaj yeem ua kom nruj ib ncig ntawm lub raj qhov kawg thiab lub ntsej muag tubesheet. Qhov clamp no compresses lub gasket los yog lub PTFE raj flare tiv thaiv tubesheet, ib ntus sealing qhov sib koom ua ke.
Txoj kev no yog qhov "kawg kawg" kho vim tias:
Nws yuav tsum tau ib tug clamp tshwj xeeb tsim rau lub raj txoj kab uas hla thiab tubesheet geometry.
Installation yog complex dua plugging.
Lub clamp tuaj yeem cuam tshuam nrog cov raj uas nyob ib sab yog tias lub suab nruj.
Nws tsis tshua muaj kev ntseeg siab tshaj qhov ntsaws thiab yuav loosen nrog thermal cycling.
Hauv kev xyaum, lub raj ntsaws yog yuav luag ib txwm nyiam. Yog tias qhov xau ntawm qhov sib koom ua ke thiab kev sib txuas tsis tuaj yeem ua tau vim tias ob qho kawg tsis tuaj yeem nkag mus tau lossis lub raj yuav tsum nyob twj ywm hauv kev pabcuam, qee lub tuam txhab kho tshwj xeeb tuaj yeem txhim kho lub raj hauv ob sab phlu lossis lub welded thaj, tab sis qhov ntawd dhau mus dhau qhov xwm txheej ceev.
Dab tsi tuaj yeem Plugged: Plhaub -Side Leaks
Cov txheej txheem tau piav qhia saum toj no tsuas yog ua haujlwm thaum lub xau tso cai rau cov kua dej dhaulos ntawm lub raj sab mus rau lub plhaub sab. Yog hais tias cov dej ntws tawm los ntawm lub plhaub tawg lossis lub plhaub ua tsis tiav - sab gasket - tso cai rau cov cua txias kom khiav tawm mus rau sab nraud - raj ntsaws tsis muaj kev kho. Plhaub- sab xau yuav tsum tau depressurization, ntws, thiab hloov gasket los yog plhaub vuam. Hauv cov xwm txheej zoo li no, kev kaw qhov xwm txheej ceev tsis tuaj yeem zam tau.
Ib yam li ntawd, yog tias lub raj PTFE tau tawg los yog sib cais raws qhov ntev, ntsaws ob qhov kawg yuav tsum tsis txhob ntws los ntawm lub raj ntawd, tab sis qhov sib cais nws tus kheej tuaj yeem tso cai hla - kis kab mob yog tias lub raj tseem nyob nrog lub plhaub - sab dej. Qhov no yog qhov lees txais yog tias lub raj xaus tau ntsaws thiab lub raj tau zoo tuag- xaus; Txawm li cas los xij, cov kua dej uas seem hauv lub raj txuas tuaj yeem ua rau corrosion lossis khov puas thaum lub sijhawm. Qee tus neeg ua haujlwm xaiv los sau lub raj txuas nrog cov khoom siv tsis zoo lossis cia nws qhuav.
Tom qab Kev Kub Ntxhov: Teem caij rov qab tag nrho
Kev kho mob xwm txheej ceev yog ib ntus. Cov khoom siv ntsaws yuav lub sij hawm, tab sis tam sim no lub exchanger tau poob ib co tshav kub hloov lwm lub tsev cheeb tsam, thiab cov seem ntawm cov hlab ntsha tau ntsib ib yam kev nyuaj siab uas ua rau cov thawj to. Cov hauv paus ntsiab lus (kev vibration, corrosion ntawm lub tubesheet, lossis kev tsim khoom tsis raug) yuav tsum tau hais txog ntawm qhov kev npaj ua ntej.
Lub exchanger yuav tsum tau teem rautag nrho retubingthaum ntxov tshaj plaws yooj yim kaw - feem ntau nyob rau hauv 3 mus rau 12 lub hlis, nyob ntawm seb qhov loj ntawm cov xau, tus naj npawb ntawm plugs ntsia, thiab qhov tseem ceeb ntawm cov txheej txheem. Khiav nrog ntau lub raj ntsaws rau lub sijhawm txuas ntxiv yuav ua rau muaj kev pheej hmoo ntau dhau ntawm cov hlab ntsha ntxiv. Kev khiav nrawm dua los ntawm cov kav dej qhib ntxiv tuaj yeem ua rau muaj kev yaig lossis kev vibration, ua rau cov xau ntxiv. Ib txoj cai ntawm tus ntiv tes xoo: yog tias ntau tshaj 10% ntawm cov hlab ntsaws, yuav tsum tau ua tam sim ntawd.
Thaum lub sij hawm retubing, tag nrho cov hlab yog hloov, thiab lub tubesheet qhov raug tshuaj xyuas thiab kho dua tshiab. Yog hais tias tus thawj xau yog tshwm sim los ntawm kev tsis zoo tube expansion los yog tawg tubesheet liner, cov no yog kho.
Tsim kom muaj peev xwm ntsaws qhov xwm txheej ceev
Rau cov nroj tsuag uas cia siab rau PTFE cov khoom siv hluav taws xob, ib qho kev saib xyuas zoo suav nrog:
Stocking ib txheej ntawm tapered PTFE plugsnyob rau hauv qhov ntau thiab tsawg rau txhua tus qauv exchanger ntawm qhov chaw.
Kev cob qhia cov kws kho mobnyob rau hauv cov txheej txheem plugging, nrog rau kom haum lub rooj zaum thiab kev ntsuam xyuas xau.
Documenting qhov chaw ntawm cov hlab ntsawsnyob rau hauv ib daim ntawv qhia bundle rau yav tom ntej siv.
Saib xyuas lub exchanger lub thermal kev ua tau zootom qab ntsaws kom pom thaum muaj peev xwm poob qis dua qhov kev txwv.
Hauv qee qhov chaw, tus txheej txheem kev khiav hauj lwm (SOP) rau lub raj xau teb tau muab tso rau hauv cov nroj tsuag txoj kev npaj teb xwm txheej ceev. SOP qhia txog qhov siab tshaj plaws ntawm cov raj uas tuaj yeem ntsaws ua ntej yuav tsum tau kaw.
Xaus: Tube Plugging ua thawj zaug -Aid rau PTFE Exchangers
Tube plugging yog ib qho tseem ceeb ua ntej - cov txheej txheem pab uas yuav lub sijhawm ua haujlwm, tiv thaiv kev puas tsuaj los ntawm kev kaw qhov kev puas tsuaj. Rau ibThaum muaj xwm ceev kho tubesheet xau PTFE exchanger, cov txheej txheem ua teb thawj zaug yog txhawm rau txheeb xyuas lub raj xau, tom qab ntawd cais nws los ntawm kev ntxig PTFE ntsaws rau hauv ob qhov kawg. Qhov no txwv tsis pub cov dej xau nrog tsawg kawg ntawm qhov chaw hloov pauv cua sov thiab tso cai rau cov nroj tsuag mus txuas ntxiv mus kom txog rau thaum lub sijhawm kho qhov rais tom ntej.
Lwm txoj kev sib cais-clamp muaj nyob rau hauv cov dej xau ntawm cov ntawv sib koom ua ke tab sis tsis tshua muaj kev ntseeg siab thiab tsis tshua siv. Kev ntsaws yog siv tau rau lub raj - sab xau; plhaub - sab xau feem ntau yuav tsum tau kaw tag nrho. Tom qab ntsaws, lub exchanger yuav tsum tau teem caij rau retubing, raws li khiav indefinitely nrog plugged tubes txaus ntshai overloading cov hlab seem thiab ua rau tsis ua hauj lwm ntxiv.
Kev kho thaum muaj xwm txheej ceev yog qhov tseem ceeb hauv cov khoom siv kev lag luam kev lag luam. Cov khoom siv ntsaws yooj yim, kev cob qhia cov kws tshaj lij, thiab cov txheej txheem kev txiav txim siab meej hloov qhov muaj peev xwm ua rau muaj kev puas tsuaj loj rau hauv kev tswj xyuas qhov xwm txheej. Txawm hais tias tsis muaj kev kho mob xwm txheej kub ntxhov hloov kev tsim thiab kev teeb tsa kom raug, lub raj txuas muab lub qhov rai tseem ceeb ntawm lub sijhawm xav tau los npaj kev nyab xeeb, tus nqi - raug kaw.