Ib txoj kab ntau lawm rov pib dua tom qab tau teem caij hloov kho dua tshiab. Lub tshuab hluav taws xob fluoroplastic tshiab nyuam qhuav tau teeb tsa hauv lub tank corrosive. Tsis pub dhau hnub, cov neeg ua haujlwm pom qhov tawg zoo nyob ze ntawm qhov chaw txuas. Tsis ntev tom qab, cov tshuaj lom neeg pib nkag mus. Lub tank yuav tsum tau kaw, ntws, thiab neutralized. Lub chaw ntsib kev poob qis, cov nqi tu, thiab muaj peev xwm raug kev nyab xeeb.

Lub rhaub nws tus kheej yog qhov zoo. Qhov ua tsis tiav tsis yog los ntawm tshuaj tua kab mob. Nws los ntawm kev kho tsis raug.

Hauv ib puag ncig corrosive, PTFE (polytetrafluoroethylene) cov cua sov yog qhov tseem ceeb vim lawv cov tshuaj lom neeg tshwj xeeb. Txawm li cas los xij, tsis zoo li cov cua sov hlau, lawv xav tau cov tswv yim mounting tshwj xeeb. Kev nkag siab yuav ua li cas kom ruaj ntseg lawv yam tsis muaj kev ntxhov siab yog qhov tseem ceeb rau lub sijhawm ntev -, xau- ua haujlwm dawb.

Vim li cas PTFE Mounting txawv ntawm Hlau

Hlau immersion rhaub yog mechanically nruj thiab zam clamping siab zoo. Stainless hlau los yog titanium raj tuaj yeem ruaj khov siv cov khoom siv hlau los yog cov khoom siv compression yam tsis muaj kev puas tsuaj tam sim ntawd.

PTFE coj txawv txawv. Nws muaj ntau dua coefficient ntawm thermal expansion dua hlau. Thaum rhuab, nws nthuav dav ntau dua li cov hlau tsis muaj steel lossis carbon hlau. Thaum lub caij txias, nws rov ua dua. Qhov kev nthuav dav tas mus li thiab kev sib cog lus no -paub tias yog thermal cycling- tso kev ntxhov siab rau txhua qhov kev txwv nruj.

Yog hais tias lub raj PTFE yog clamped nruj nreem nrog cov khoom siv hlau, cov khoom siv tsis muaj chaw txav. Nyob rau tib lub sijhawm, qhov kev ntxhov siab ntau ntxiv ntawm qhov taw tes clamp ua rau micro- tawg. Thaum kawg, pom cov ntaub ntawv tawg, feem ntau nyob ze ntawm flange lossis mounting interface. Hauv kev pabcuam corrosive, txawm tias qhov tawg me me tuaj yeem txhim kho sai sai rau hauv qhov xau.

Qhov teeb meem tsis yog cov khoom tsis muaj zog. Nws yog tsis tsim nyog mechanical restraint.

Tshuaj Compatibility ntawm Mounting Hardware

Mounting hardware yuav tsum phim cov tshuaj tiv thaiv ntawm lub rhaub sheath. Kev siv carbon steel brackets nyob rau hauv lub tank acid yuav ua rau corrosion. Txawm tias cov khoom siv stainless hlau tuaj yeem ua rau cov kua qaub muaj zog, ua rau muaj kab mob hauv chav da dej lossis ua kom tsis muaj zog ntawm kev txhawb nqa.

Vim li no, kev lag luam zoo tshaj plaws yog siv PTFE los yog PPS (polyphenylene sulfide) mounting brackets thiab flanges thaum ua hauj lwm nyob rau hauv cov tshuaj phem heev. Cov ntaub ntawv no muab cov tshuaj muaj zog tiv thaiv thaum tswj kom muaj zog txhua yam rau kev siv tank.

Flanges thiab brackets yuav tsum raug xaiv raws li ob qho tib si raug tshuaj lom neeg thiab kev ua haujlwm kub. Cov kab kos kev sib raug zoo thiab cov lus pom zoo ntawm tus neeg muag khoom yuav tsum ua raws li kev xaiv cov khoom siv.

Tsis txhob Rigid Hlau Clamps ntawm PTFE Tubes

Ib qho ntawm feem ntau yuam kev installation yog zawm nruj hlau clamps ncaj qha mus rau PTFE cua sov raj. Installers feem ntau xav hais tias ruaj clamping kom ruaj khov. Qhov tseeb, qhov kev xyaum no tsim cov ntsiab lus kev ntxhov siab.

Thaum lub tshuab cua sov sov, PTFE nthuav dav. Yog hais tias nws yog daig nyob rau hauv ib tug nruj clamp, internal kev nyuaj siab tsim nyob rau hauv kev sib cuag interface. Nyob rau ntau lub voj voog cua sov, kev ntxhov siab tawg tsim. Cov kab nrib pleb no feem ntau tshwm sim ntawm qhov taw tes mounting vim nws yog qhov chaw ntawm qhov siab tshaj plaws kev txwv.

Raws li kev lag luam kev paub, clamps yuav tsum tsis txhob ncaj qha mus rau PTFE sheath. Yog tias xav tau kev txhawb nqa ntxiv, nws yuav tsum tsim kom muaj kev txav mus los.

Lub luag haujlwm ntawm Floating Flanges

Floating flanges yog dav siv los ua kom haum thermal expansion. Tsis zoo li cov flanges ruaj khov, cov qauv tsim ntab tso cai rau me ntsis axial txav ntawm lub rhaub dej thaum lub sij hawm thermal cycling.

Hauv kev xyaum, lub flange ruaj ntseg lub rhaub ntawm lub tank phab ntsa thaum tso cai rau kev nthuav dav raws qhov ntev ntawm lub raj. Qhov no txo ​​cov neeg kho tshuab kev nyuaj siab thiab khaws cov qauv kev ntseeg siab.

Gaskets siv ntawm flange interface yuav tsum tau chemically tshaj thiab compressed tusyees. Tshaj -tightening flange bolts tuaj yeem cuam tshuam cov khoom PTFE, tshwj xeeb tshaj yog nyob rau hauv cov phab ntsa yas tank. Bolts yuav tsum tau nruj nruj nyob rau hauv ib tug ntoo khaub lig qauv nrog tswj torque.

Adjustable Mounting Ncej rau cov tank loj dua

Hauv qhov qhib loj dua - cov tso tsheb hlau luam sab saum toj, cov tshuab tso cua sov tuaj yeem txuas ntxiv mus rau hauv chav da dej. Txhawm rau tiv thaiv kev vibration lossis kev sib cuag nrog lub tank phab ntsa, feem ntau yuav tsum muaj kev txhawb nqa.

Es tsis txhob thav duab nruj, adjustable mounting systems raug pom zoo. Cov thav duab no muab kev taw qhia thiab qhov chaw ruaj ntseg yam tsis txwv kev nthuav dav. Lub tshuab cua sov tuaj yeem txav me ntsis raws li qhov kub hloov pauv, tsis txhob muaj kev ntxhov siab.

Cov ntsiab lus txhawb nqa yuav tsum siv cov tshuaj tiv thaiv eeb lossis cov lus qhia es tsis yog cov clamps nruj. Clearance nruab nrab ntawm lub rhaub thiab tank phab ntsa yuav tsum tau tswj kom tsis txhob muaj kev sib cuag thaum lub sij hawm nthuav.

Kev txiav txim siab rau ntau hom Tank

Mounting tswv yim txawv nyob ntawm seb lub tank configuration.

Qhib- cov tso tsheb hlau luam sab saum toj feem ntau siv tshaj -- cov cua sov sab uas muaj kev ruaj ntseg nrog cov hlua khi rau ntawm ntug tank. Hauv qhov no, kev nthuav dav feem ntau yog qhia kab rov tav, thiab qhov chaw txaus yuav tsum tau tso cai rau kev txav mus los.

Hauv qhov sib piv, kaw lossis cov hlab ntsha uas muaj zog yuav tsum tau flange -mounted immersion heaters. Nyob rau hauv cov txheej txheem no, sealing kev ncaj ncees ua ib qho tseem ceeb. Kev xaiv gasket kom zoo, tswj lub zog, thiab kev tso cai rau thermal txav yog qhov tseem ceeb los tiv thaiv kev xau.

Pressurized systems xav tau ntau dua precision vim hais tias txhua yam kev nyuaj siab ua ke nrog rau sab hauv siab zog. Kev ntsuam xyuas kev tshaj lij engineering tau pom zoo rau hauv cov xwm txheej no.

Installation Cov kev coj ua zoo tshaj plaws

Txhawm rau kom tsis txhob tawg thiab tawg, cov hauv paus ntsiab lus hauv qab no yuav tsum qhia kev teeb tsa:

Siv cov tshuaj sib xyaw ua ke PTFE lossis PPS mounting kho vajtse.

Tsis txhob ncaj nraim clamping ntawm PTFE sheath.

Cia qhov chaw rau thermal expansion thiab contraction.

Siv cov flanges uas tsim nyog.

Tighten flange bolts tusyees thiab kom pom zoo torque qhov tseem ceeb.

Tswj kom zoo tshem tawm ntawm cov phab ntsa tank thiab cov txheej txheem sab hauv.

Cov kauj ruam no yuav tshwm sim yooj yim, tab sis saib ib qho ntawm lawv tuaj yeem ua rau ua tsis tiav ntxov.

Tiv thaiv kev ncaj ncees los ntawm kev kho kom raug

PTFE cua sov muab cov tshuaj tiv thaiv zoo heev hauv cov txheej txheem kev lag luam hnyav. Txawm li cas los xij, lawv tus cwj pwm mechanical txawv heev ntawm cov khoom siv hlau. Kev kho kom raug tsis yog qhov nthuav dav me me - nws yog qhov tseem ceeb rau kev ntseeg tau ntawm lub cev.

Ib qho tawg mounting point tsis tsuas cuam tshuam kev tsim khoom tab sis kuj tsim kev nyab xeeb kev nyab xeeb nyob rau hauv ib puag ncig corrosive. Kev tiv thaiv tsis zoo li no yuav tsum tau nkag siab txog kev nthuav dav thermal, xaiv cov khoom siv sib xws, thiab tsim kom muaj kev txav mus los tsis yog kev txwv.

Cov kev teeb tsa lub tank sib txawv-txawm yog qhib- cov tshuaj da dej saum toj kawg nkaus lossis cov hlab ntsha siab tshaj - yuav tsum tau tsim cov tswv yim txhim kho. Kev ntsuam xyuas ntawm lub tank layout thiab kev khiav hauj lwm tej yam kev mob ua kom paub tseeb tias lub rhaub nyob ruaj ntseg, saj zawg zog, thiab xau- dawb nyob rau hauv lub sij hawm ntev.

Nyob rau hauv daim ntawv thov cua sov corrosive, ua tib zoo mounting khaws cia ob qho tib si khoom siv thiab kev nyab xeeb ntawm kev ua haujlwm.