PTFE cua sov daim hlau muaj nuj nqis rau lawv cov tshuaj tiv thaiv, hluav taws xob rwb thaiv tsev, thiab thermal stability. Hauv ntau qhov chaw ua lag luam thiab kev tshawb fawb, cov khoom zoo no ua rau lawv cov neeg sib tw txaus nyiam siv rau hauv lub tshuab nqus tsev, suav nrog lub tshuab nqus tsev vacuum, lub tshuab ziab khaub ncaws khov, lossis qis - cov txheej txheem siab. Txawm li cas los xij, kev khiav hauj lwm PTFE cua sov phaj hauv lub tshuab nqus tsev qhia txog cov teeb meem tshwj xeeb uas tsis tau ntsib nyob rau hauv huab cua. Cov kws kho tsheb yuav tsum nkag siab tias cov khoom siv coj li cas nyob rau hauv qhov tsis tshua muaj siab, hloov cov cua sov li cas, thiab qhov kev hloov kho uas tsim nyog rau kev lag luam txhim khu kev qha.
Outgassing kev txiav txim siab
Ib qho kev txhawj xeeb tseem ceeb rau cov polymers hauv lub tshuab nqus tsev yog outgassing. PTFE, zoo li tag nrho cov polymers, muaj cov pa roj nkag thiab cov khoom tsis sib haum xeeb uas tuaj yeem tso tawm thaum raug rau qis - qhov chaw siab. Hauv cov ntawv thov rhiab xws li nyias - zaj duab xis tso tawm lossis ua cov khoom siv semiconductor, txawm tias cov pa tawm me me tuaj yeem ua rau cov txheej txheem, txo cov khoom zoo, lossis tso cov yeeb yaj kiab tsis xav tau rau ntawm qhov chaw tseem ceeb.
Qhov tsawg kawg nkaus outgassing yuav tsum tau siv high -purity, nqus{1}} ci PTFE qib. Ua ntej- ci tshem tawm cov khoom seem thiab cov dej noo, txo qhov kev pheej hmoo ntawm kev sib kis. Cov kws tshaj lij qhia cov phiaj xwm cua sov rau kev pabcuam lub tshuab nqus tsev yuav tsum paub meej tias cov khoom siv thiab cov nplaum siv hauv cov phaj yog tsim rau qis- qhov chaw siab, vim qee qhov sib txuas cov neeg ua haujlwm lossis cov khoom siv hauv lub davhlau ya nyob twg tuaj yeem outgas ntau dua li PTFE nws tus kheej.
Nyob rau hauv kev xyaum, tus qauv PTFE cua sov phaj tsim rau atmospheric siv tau tso pa txaus nyob rau hauv lub nqus tsev vacuum los cuam tshuam cov txheej txheem rhiab heev. Lub tshuab nqus tsev- cov phaj ci yog li ntawd ib qho kev daws teeb meem, kom ntseeg tau tias cov khoom seem seem raug tshem tawm ua ntej kev teeb tsa.
Thaum tshav kub kub hloov nyob rau hauv qis siab
Thermal cwj pwm kuj hloov hauv lub tshuab nqus tsev. Ntawm atmospheric siab, convective heat transfer plays lub luag haujlwm tseem ceeb hauv kev txav cua sov ntawm lub phaj mus rau ib puag ncig ib puag ncig. Nyob rau hauv lub tshuab nqus tsev, convection yog qhov tseem ceeb tshem tawm, tawm tsuas yog conduction los ntawm cov khoom sib txuas thiab hluav taws xob hloov hluav taws xob. Cov kws kho tsheb yuav tsum suav rau qhov txo qis ntawm cov cua sov no, vim tias qhov chaw uas tshwm sim kom ncav cuag qhov xav tau ntawm qhov kev xav tau nyob rau hauv ib txwm muaj siab yuav overheat hauv lub tshuab nqus tsev.
Kev xav txog kev tsim qauv suav nrog kev ua kom muaj kev sib raug zoo ntawm PTFE phaj thiab cov khoom thauj los yog qhov chaw sib txuas kom ua kom cov hluav taws xob hloov pauv ntau tshaj plaws. Radiative tshav kub poob tuaj yeem tswj tau los ntawm kev xaiv cov emissive coatings los yog cov ntaub thaiv npog raws li qhov tsim nyog. Cov tswv yim tswj qhov kub thiab txias tuaj yeem xav tau ntau qhov kev txuag ramp tus nqi thiab cov lus tawm tswv yim uas suav nrog kev hloov pauv thermal dynamics hauv lub tshuab nqus tsev.
Mechanical Stability
PTFE yog mechanically ruaj khov nyob rau hauv ib txwm tej yam kev mob, tab sis lub nqus tsev vacuum yuav qhia ntxiv kev nyuaj siab. Tej huab cua los yog voids nyob rau hauv lub PTFE los yog lub rooj sib txoos tuaj yeem nthuav dav thaum lub siab nyob ib puag ncig poob, uas yuav ua rau micro- tawg lossis delamination. Txawm tias muaj kev pheej hmoo tsawg rau cov khoom, siab - cov phaj zoo, qhov tseem ceeb no qhia txog qhov tseem ceeb ntawm kev qhia ntom ntom, tsis muaj dab tsi - cov ntaub ntawv pub dawb thiab tsis txhob muaj kab noj hniav nyob hauv qhov tsim.
Tsis tas li ntawd, qhov sib txawv thermal expansion ntawm PTFE thiab mounting lossis cov ntaub ntawv txhawb nqa tuaj yeem ua kom pom tseeb hauv lub tshuab nqus tsev, tshwj xeeb tshaj yog thaum ua haujlwm kub -. Saj zawg zog los yog slotted mounting systems pab haum rau expansion thiab contraction tsis inducing mechanical stress.
Hluav taws xob rwb thaiv tsev thiab Terminal Design
PTFE tuav zoo heev dielectric zog nyob rau hauv lub tshuab nqus tsev vacuum. Txawm li cas los xij, qis - cov kev mob siab tuaj yeem ua rau muaj qhov tshwm sim ntawm corona tawm lossis arcing ntawm cov npoo ntse lossis cov khoom siv tsis zoo. Kev sib txuas hluav taws xob yuav tsum tau tsim kom muaj qhov sib txawv txaus, cov khoom sib npaug, thiab lub tshuab nqus tsev- siv cov ntaub ntawv insulating los tiv thaiv hluav taws xob tsis ua haujlwm.
Kev taw qhia tswv yim suav nrog kev siv cov xaim hlau kaw, lub tshuab nqus tsev- sib xyaw potting compounds, thiab xyuas kom meej tias cov khoom siv hluav taws xob tiv thaiv los ntawm kev raug rau lub chamber sab hauv.
Qhia meej txog lub tshuab nqus tsev-Compatible PTFE Heating Phaj
Thaum xaiv PTFE cua sov daim hlau rau daim ntawv thov lub tshuab nqus tsev, ntau qhov kev txiav txim siab kom ntseeg tau tias kev ua haujlwm zoo:
Kev xaiv khoom siv:Siv siab -purity, nqus tsev vacuum- ci PTFE kom txo tau cov pa tawm.
Mounting tsim:Muab qhov hloov tau yooj yim lossis slotted mounting kom haum rau thermal expansion thiab contraction.
Kev tswj cov cua sov:Xyuas kom zoo conductive sib cuag thiab xav txog radiative tshav kub hloov, vim convection tsis tuaj.
Hluav taws xob tsim:Rwb thaiv tsev terminals thiab ua rau tiv thaiv corona tawm, siv lub tshuab nqus tsev -cov khoom sib xws.
Kev txheeb xyuas cov txheej txheem:Paub meej tias cov cua sov phaj qhov tawm ntawm qhov hluav taws xob thiab thermal kev ua tau zoo yog sib xws nrog lub rhiab heev ntawm lub tshuab nqus tsev.
Hauv kev xyaum, kev sab laj nrog cov chaw tsim khoom txog lub tshuab nqus tsev- cov phaj ntsuas yog qhov tseem ceeb. Cov kws tshaj lij tuaj yeem muab cov chav tsim tshwj xeeb rau kev ua haujlwm siab - qis, suav nrog lub tshuab nqus tsev- cov khoom ci, cov khoom siv hluav taws xob kaw, thiab kev txhim kho kev txhim kho kom zoo.
Xaus
PTFE cua sov phaj tuaj yeem ua haujlwm tau zoo hauv lub tshuab nqus tsev thiab qis- qhov chaw siab, tab sis cov qauv tsim huab cua yuav tsis haum. Outgassing, hloov pauv cov cua sov, kev ntxhov siab, thiab hluav taws xob xav tau txhua yam yuav tsum tau ua tib zoo saib xyuas. Nrog rau kev xaiv cov khoom tsim nyog, tsim kev hloov kho, thiab kev teeb tsa, PTFE cua sov daim hlau tuaj yeem muab kev ua haujlwm thermal txhim khu kev qha thaum tswj kev ncaj ncees ntawm cov txheej txheem nqus tsev. Rau cov ntawv thov tseem ceeb, kev koom tes nrog cov tuam txhab lag luam uas paub txog hauv lub tshuab nqus tsev kom paub meej tias cov phaj cua sov ua tau raws li cov kev xav tau nruj ntawm kev ua haujlwm siab tsawg -.