Hauv cov chaw soj ntsuam kev tshawb fawb thiab cov chaw tshwj xeeb hauv kev lag luam, kev sib pauv cua sov nrog cov xov xwm txawv txawv tiag tiag nthuav tawm cov teeb meem loj heev. Molten ntsev rau thermal zog cia, kua gallium nyob rau hauv siab txias loops, concentrated hydrogen peroxide nyob rau hauv propellant ua, los yog molten sulfur nyob rau hauv sulfur rov qab units thawb cov pa cov ntaub ntawv tshaj lawv cov kev txwv. Stainless hlau, Hastelloy, titanium, thiab txawm iav - cov khoom siv lined feem ntau corrode sai, embrittle, los yog catalyze yam tsis xav tau. PTFE's unparalleled tshuaj inertness ua rau nws yog ib tug txaus nyiam neeg sib tw, tab sis nws haum rau cov aggressively, siab -kub, los yog reactive heev reactive fluids nyob deb ntawm universal. Cov kws tshawb fawb tshawb fawb thiab cov kws tsim tshuaj tshwj xeeb xav tau kev taw qhia meej txog qhov twg PTFE ua tau zoo thiab qhov twg cov kev txwv tseem ceeb tshaj tawm lwm txoj hauv kev.

Molten ntsev

Ntau cov ntsev molten-xws li hnub ci ntsev (NaNO₃-KNO₃) los yog chloride-raws li kev sib xyaws- ua haujlwm ntawm 300–600 ° C, zoo tshaj PTFE qhov kev ua haujlwm tsis tu ncua ntawm kwv yees li 260 ° C (thiab feem ntau derated rau 200 ° C rau 200 ° C). Ntawm cov kub no, PTFE degrades los ntawm saw scission, volatilization, thiab creep loj heev. Tsawg- cov ntsev yaj, txawm li cas los xij, poob hauv qhov ncav cuag. Eutectic sib tov nrog cov ntsiab lus melting hauv qab 150 ° C (xws li, qee cov nitrate lossis organic ntsev sib tov) tso cai rau PTFE cov khoom siv hluav taws xob ua haujlwm, muab qhov kub thiab txias qis dua cov khoom muaj kev nyab xeeb. Qhov kev txhawj xeeb tseem ceeb hloov los ntawm thermal degradation mus rau mechanical abrasion. Solidified ntsev hais los yog undissolved impurities tuaj yeem nplawm PTFE nto thaum lub sij hawm pib, txias, los yog ntws transients, tsim micro- khawb uas ua kom fouling los yog pib kev ntxhov siab tawg. Nyob rau hauv kev xyaum, PTFE tshav kub exchangers tau ntse siv nyob rau hauv molten sulfur daim ntaub ntawv mus txog 150 degrees Celsius, tab sis cov neeg kho tshuab puas los ntawm cov khoom hais yog teeb meem ntau tshaj li tshuaj tua kab mob.

Cov hlau ua kua

PTFE ua kom pom kev ua haujlwm zoo rau ntau cov kua hlau ntawm qhov kub nruab nrab. Mercury thiab gallium- siv rau hauv qhov tshwj xeeb txias txias lossis cua sov hloov lub voj voog - ua rau muaj kev cuam tshuam tsis zoo hauv qab 150-200 ° C. Kev ntub dej tsis zoo, thiab qhov nro saum npoo txwv kev nkag mus rau hauv micro- tsis xws luag. Txawm li cas los xij, reactive alkali hlau xws li molten sodium, potassium, los yog sodium -poov tshuaj alloys hnov ​​​​mob hnyav nrog PTFE. Defluorination tshwm sim sai, ua kom sov, carbonaceous residue, thiab muaj peev xwm ignition txaus ntshai. Txawm tias cov kab mob alkali hlau paug nyob rau hauv lwm yam inert systems tuaj yeem pib tawm tsam hauv zos. Compatibility yog li ntawd nyob ntawm ntau yam ntawm cov hlau thiab kub; Tsis muaj kev pom zoo dav dav rau cov hlau alkali.

Muaj zog Oxidizers thiab Halogens

Concentrated hydrogen peroxide (>70%), ozone-saturated solutions, chlorine dioxide, thiab lwm yam muaj zog oxidizers ua rau qeeb tab sis muaj kev hem thawj. Ntawm qhov kub thiab txias, PTFE tiv taus cov xov xwm no zoo, tab sis qhov kub siab ua kom oxidative saw scission, ua rau kom tawv nqaij dawb, embrittlement, thiab nws thiaj li tawg. Qhuav elemental halogens nthuav qhia txoj kab sib faib. Dilute aqueous chlorine, bromine, los yog iodine cov kev daws teeb meem feem ntau sib xws, tab sis cov roj fluorine qhuav -txawm yog nyob rau hauv chav tsev kub -reacts heev, tsim volatile perfluorocarbons thiab ua rau yaig sai heev. Chlorine trifluoride coj zoo ib yam. Aqueous lossis sib xyaw-theem halogen kwj feem ntau nyob nyab xeeb hauv qhov kub thiab txias.

Qhov tseem ceeb ntawm kev xeem daim coupon thiab daim ntawv thov validation

Rau ib qho kev sib txawv nruab nrab-tshwj xeeb yog cov qauv tshiab lossis cov khoom sib xyaw ua ke- tsis tuaj yeem xav tau los ntawm cov kab kos lossis cov ntaub ntawv. Kev kuaj daim coupon tshwj xeeb muab cov ntaub ntawv txhim khu kev qha xwb. Tshaj tawm cov qauv PTFE me me (xws li txiav los ntawm tib qib thiab tuab raws li qhov xav tau ntawm cov raj xa dej) mus rau cov txheej txheem dej hauv cov neeg sawv cev: kub, siab, ntws nrawm, thiab ntev (lub lis piam mus rau hli). Ntsuas cov txiaj ntsig los ntawm:

Kev hloov pauv hnyav (nce los ntawm kev nqus lossis poob los ntawm degradation)

Kev soj ntsuam pom (dawb, tawg, blistering, discoloration)

Mechanical xeem (lub zog tensile, elongation, hardness)

Kev soj ntsuam saum npoo (microscopy, FTIR rau tshuaj hloov pauv)

Ib txoj hauv kev rau cov ntawv thov tshiab tiag tiag yog ua daim coupon xeem nthuav tawm ib qho me me ntawm PTFE rau cov txheej txheem tiag tiag rau ob peb lub lis piam ua ntej cog lus rau kev sib pauv pauv tag nrho. Cov txiaj ntsig tau zoo- qhov hloov pauv qhov hnyav tsawg (<0.5%), no visible attack, retained mechanical properties-support proceeding; measurable degradation or unexpected behavior demands reevaluation or alternative materials.

PTFE tuaj yeem lis qee yam kab txawv tshaj tawm zoo, tab sis nws tsis yog qhov kev daws teeb meem thoob ntiaj teb. Kev txwv qhov kub thiab txias, mechanical abrasion, oxidative attack, thiab kev ua phem rau cov hlau reactive ua rau nruj ciam teb. Daim ntawv thov nruj nruj los ntawm kev kuaj daim coupon tseem tseem ceeb rau cov kev pabcuam uas tsis tau lees paub.

Rau cov ntawv thov nyuaj tshaj plaws, koom tes nrog cov chaw tsim khoom uas tuaj yeem muab daim coupon xeem, ua cov kev tshawb fawb raug tswj, thiab muab cov kev ntsuam xyuas tsis ua haujlwm yog txoj hauv kev nyab xeeb tshaj plaws rau kev ua tiav, kom ntseeg tau tias qhov kev xaiv sib pauv tsim tiag tiag phim cov kev xav tau ntawm cov kab txawv nruab nrab.